2003-10-21
delphine meunier
2003-10-21
Hong Wu
sintering of aluminum
Hong Wu
2003-10-21
Al/Si sintering is 400C-430C. I don't know what sintering you talking about.

Hong Wu


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
delphine meunier
Sent: Tuesday, October 21, 2003 8:56 AM
To: [email protected]
Subject: [mems-talk] sintering of aluminum


Dear all,

Did you know the procedure of aluminum sintering? Temperature (I supposed
660°C, melting point)? Time??

Thanks,

Delphine Meunier
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Addison Engineering