MEMSnet Home: MEMS-Talk: Wafer temperature measurements
Wafer temperature measurements
1997-11-17
Ram N. Ramanan
1997-11-20
Ram N. Ramanan
Wafer temperature measurements
Ram N. Ramanan
1997-11-20
Dear Colleagues,

Does anyone know of companies that sell wafers with thermocouples
or RTD attached on them (& boards for data acquisition). I know
of only one (sensarray)... Are there any other companies that
do this ?

Thanks in advance,
Ram
 --

--
*********************  Ram N. Ramanan *******************************
FSI International,  MS 5-7060, 600 Millennium Drive, Allen, TX-75013
Ph: 972-643-2213 [email protected] (w); [email protected] (H)
www: http://www.fsi-intl.com
********************************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.