Dry etching of Platinum
2003-11-14
Raj Kumar
2003-11-14
Bill Moffat
Dry etching of Platinum
Bill Moffat
2003-11-14
Think image reversal, metal lift off, and dimensions down to 0.1 micron.  Bill
Moffat

-----Original Message-----
From: Raj Kumar [mailto:[email protected]]
Sent: Thursday, November 13, 2003 10:06 PM
To: [email protected]
Subject: [mems-talk] Dry etching of Platinum



Hello Friends!
       I was looking for some dry etch recipe for patterning Platinum
with 1 micron dimensions. In addition to that I was also looking for the
stability of Platinum in KOH and TMAH based wet anisotropic etching. Any
guideline and/or reference in this context will be highly appreciated.

Rajkumar,India


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing