MEMSnet Home: MEMS-Talk: zinc oxide ZnO and metals
zinc oxide ZnO and metals
2003-11-18
Steven F. Nagle
2003-11-18
Shweta Humad
2003-11-19
Jim Intrater
2003-11-19
Steven F. Nagle
zinc oxide ZnO and metals
Jim Intrater
2003-11-19
Are you sputtering the Pt? If so, you should sutter an adhesion layer of Cr.
----- Original Message -----
From: "Steven F. Nagle" 
To: 
Sent: Monday, November 17, 2003 6:04 PM
Subject: [mems-talk] zinc oxide ZnO and metals


> Can anyone tell me several metals that adhere well to zinc oxide?  More
> specifically, would we need an adhesion layer for Pt?
>
> Thanks.
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics