MEMSnet Home: MEMS-Talk: Simple Young's Modulus for Silicon... Please
Simple Young's Modulus for Silicon... Please
2003-11-25
Pete Crompton
2003-11-26
Imran Ghauri
Diamond
2003-11-26
VIKAS
2003-11-26
Imran Ghauri
2003-11-26
RobDavis
2003-11-28
Jim Intrater
2003-12-01
David Nemeth
2003-11-26
Yilei Zhang
Simple Young's Modulus for Silicon... Please
Imran Ghauri
2003-11-26
First of all Young's modulus for Si can be chosen from
120 to 170. It depends upon many paramters like
deposition rate, temperature, pressure, residual
stresses, intrinsic stresses and thermal stresses and
of course it will be different for different
structures. It also depends upon the stiffness of the
material that you are using for your application. Also
geometry too. So you can see there are so many things
that determine the YOungs' modulus of Si. So you can
select about some value between what I've suggested in
the beginning. Good luck
Imran
--- Pete Crompton  wrote:
> Hello.
>
> My name is Peter Crompton. I am a Sixth Form student
> currently studying at
> Carmel College in Merseyside, England. I have
> coursework to do on Silicon
> and I was wondering if anyone could help me with the
> Young's Modulus of
> Silicon. It would be helpful if it was quite simple
> and if anyone could
> explain why there are so many variations of the
> Young's Modulus for Silicon
> that would also be a great help.
>
> Thankyou Very Much, Peter Crompton
>
>
_________________________________________________________________
> Find a cheaper internet access deal - choose one to
> suit you.
> http://www.msn.co.uk/internetaccess
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________
Do you Yahoo!?
Free Pop-Up Blocker - Get it now
http://companion.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics