MEMSnet Home: MEMS-Talk: PZT in microphone applications
PZT in microphone applications
2003-12-03
Zheyao Wang
2003-12-03
Wieslaw Bicz
PZT in microphone applications
Wieslaw Bicz
2003-12-03

Zheyao Wang wrote:

> Dear All,
>
> There are several papers on using piezoelectric materials, such as ZnO and
PVDF,
> in audio frequency microphone applications. Since it is evident that PZT has
superior
> features to ZnO and PVDF, why there is no one to use PZT in audio microphones?
> Are there some fatal disadvantages determining that PZT is not possible in
audio
> applications?
>

There may be some reasons:

1. Impedance too high.
2. Necessary thickness for audio frequencies is too large.
3. But probably the most important reason is: electret membrane microphones are
easier to make,
cheaper etc.

I think, that it would be possible to use PZT in microphones, but somebody must
propose an idea,
that would work properly. If this makes sense is open question.


Wieslaw Bicz

---------------==========   OPTEL sp. z o.o.   ===========---------------
------===== R&D: Ultrasonic Technology/Fingerprint Recognition ====------
ul. Otwarta 10a PL 50-212 Wroclaw Tel.:+48 71 3296854 Fax.:+48 71 3296852
--------==== mailto:[email protected]  -=-  http://www.optel.pl ====-------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering