MEMSnet Home: MEMS-Talk: Flexus F-5000 Film Stress Gauge
Flexus F-5000 Film Stress Gauge
2003-12-16
[email protected]
2003-12-18
Phillipe Tabada
Flexus F-5000 Film Stress Gauge
Phillipe Tabada
2003-12-18
Hi Bob,

   I believe UC Berkeley has a flexus, but I am not quite sure if its the
exact model.  I would recommend calling them up and ask for Bob Hamilton at
(510) 642-2716.

Phil Tabada


>From: [email protected]
>Reply-To: General MEMS discussion 
>To: [email protected]
>Subject: [mems-talk] Flexus F-5000 Film Stress Gauge
>Date: Tue, 16 Dec 2003 12:24:47 -0500
>
>Does anyone within the MEMS community have access to a Flexus Films stress
>gauge F-5000? The product has been discontinued and I have need to find one
>that is in working condition. Please contact me directly if you have one or
>know of someone that does. Thanks  Bob Henderson 602-206-6154
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Working moms: Find helpful tips here on managing kids, home, work —  and
yourself.   http://special.msn.com/msnbc/workingmom.armx



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer