Hi

Actually, I spined a PDMS layer on a SI wafer. After curing, I need to transfer
my pattern on the PDMS layer by gold deposition and using lift off process.Can I
make my pattern by photoresit and then evaporate gold? Is there any special
recepie?

Best regards,
Hasan Sharifi