Shay Kaplan
2004-01-02
this is done in perspex manufacturing all the time. Crosslinking by UV is a
lhithogaphers invention.
shay

Oluwasijibomi Okeowo wrote:

> Anyone has an idea on the possibility of crosslinking PMMA using organic
peroxides?
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing