Hello,

   Has anyone dealt with the gold thinfilm behavior
during high tempture before? I know the Au thinfilm
will turn into very small gold particles at high
tempture. I am trying to figure out the relationship
between the particle size and thickness of Au layer.

Thanks,
Chun-I

__________________________________
Do you Yahoo!?
Yahoo! Hotjobs: Enter the "Signing Bonus" Sweepstakes
http://hotjobs.sweepstakes.yahoo.com/signingbonus


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Harrick Plasma, Inc.
University Wafer