High volume thin film deposition systems
2004-01-14
[email protected]
High volume thin film deposition systems
[email protected]
2004-01-14
 Hi Everybody,

  I am looking for sputter/E-beam deposition systems that can do high volume
AR( Anti-reflection) coatings for our plastic lens components. We are
typically looking at a turnaround of 12000 - 15000 miniature lenses ( 1 -3
mm diameter)per day. I would greatly appreciate if anybody is aware of an
existing system that could potentially do this.

 Best Regards
Sreeram Appasamy
Applied Image Group Optics
[email protected]
520-806 3844


----------------------------------------------------------------------------
----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------

This email, including attachments, contains information that is privileged,
confidential or subject to non-disclosure agreements or intellectual
property laws.  This email, including attachments, constitutes non-public
information intended to be conveyed only to the designated recipient(s).  If
you are not the intended recipient, please delete this email, including
attachments, and notify the sender by return mail, email, or by calling (ALL
CONTACT INFORMATION LISTED BELOW). The unauthorized review, use,
dissemination, distribution, or reproduction of this email, including
attachments, is prohibited and may be unlawful.

APPLIED IMAGE Group / Optics subsidiary
4400 South Santa Rita Avenue
Tucson, AZ 85704
phone:  520-806-3800
fax:    520-806-3899

----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------
----------------------------------------------------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group