overhanging
1997-02-15
Mr Philippe HELIN
overhanging
Mr Philippe HELIN
1997-02-15
Does anyone know how to make an overhanging using two photoresists to =
realize a lift-off.
Could you please inform me on the followings :
* Photoresists, manufacturer
* exposure time, wavelength
* remover
* and so on

Thanks

Philippe HELIN
IEMN
Avenue Poincar=E9, BP 69
59652 Villeneuve d'Ascq, FRANCE
fax : 333 20 19 78 78
Email : [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.