Dear MEMS group!

I want to compare different machining processes with respect to their surface
quality (surface roughness!). Can anyone provide rough data or even a scientific
reference on the surfce roughness of SU-8? Is there a difference on the
horizontal planes and the vertical sidewalls?

How good is the surface quality of SU-8 compared with other machining techniques
such as UV/X-ray LIGA or electroforming?

Any help and any hint will be greatly welcomed!

Stephan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer