A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quickly dissolving thick PMMA
Quickly dissolving thick PMMA
2004-02-02
Hunter, Luke L
2004-02-02
Karl Cazzini
2004-02-02
Narayanan Unni
2004-02-02
William Lanford-Crick
2004-02-03
Michael D Martin
2004-02-03
Greg Miller
2004-02-03
Gary
2004-02-04
Michael L
2004-02-04
Hunter, Luke L
Quickly dissolving thick PMMA
Hunter, Luke L
2004-02-04
Thanks for all the good suggestions.  The PMMA that's being dissolved is a
LIGA mold with metal parts in it, so we'll want to try things that won't
attack metal.  Co-workers are trying a few things now and I'll post results
once we know more.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.