MEMSnet Home: MEMS-Talk: n-doped or p-doped GaAs wet chemically etches well?
n-doped or p-doped GaAs wet chemically etches well?
2004-02-06
Sai Raghav Parasa
n-doped or p-doped GaAs wet chemically etches well?
Sai Raghav Parasa
2004-02-06
Hi,

Can anyone of you tell me whether n-doped or p-doped GaAs wet chemically etches
well with the etchant Citric acid:H2O (50g:50ml):H2O2 (10ml) or with the etchant
[Citric acid:H2O (1:1)]:H2O2 (1.5:1) ?

Thank you very much,
Bye,
Parasa.







---------------------------------
Do you Yahoo!?
Yahoo! Finance: Get your refund fast by filing online
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing