MEMSnet Home: MEMS-Talk: Preparation of KI+I2+DIwater solution for gold etching
Preparation of KI+I2+DIwater solution for gold etching
2004-02-08
hare krishna
2004-02-09
aasutosh dave
SU8 Information
2004-02-10
[email protected]
2004-02-10
Samir Kagadkar
SU-8 adhesion problem
2004-02-11
[email protected]
2004-02-11
Karin Buchholz
2004-02-12
Greg Reimann
Polishing service
2004-02-16
Changping LUO
2004-02-10
hare krishna
TLM structure for measuring the specific contact resistance
2004-02-11
hare krishna
2004-02-16
aasutosh dave
Preparation of KI+I2+DIwater solution for gold etching
hare krishna
2004-02-08
Dear All,
             How should I make the solution of KI + I2 + DI water for the gold
etching. Should I use it fresh or I can use it for long time...and how should it
be preserved.
Regards
Hare Krishna



Yahoo! India Education Special: Study in the UK now.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation