Low stress thermal oxide? Tensile stress?
2004-02-13
Zhimin J Yao
2004-02-27
Steven F. Nagle
Low stress thermal oxide? Tensile stress?
Zhimin J Yao
2004-02-13
Hello,

Can anyone grow thermal oxide with a very low compressive stress (<10 MPa)
or tensile stress?  I need about 1 um of SiO2 on 4 inch Si wafers.  It is
OK if H2 or some other elements needed to be introduced into the film.

Any information leads to finding a vendor is greatly appreciated.

Zhimin





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation