Would anyone know how thin of a layer of silver can I deposit on glass
that will still reflect a 325nm UV wavelength. I've done some research,
but I can not find an absolute answer. I believe its somewhere below
300nm though.

Thank you for any suggestions,
Ed Keough


reply