MEMSnet Home: MEMS-Talk: Resistance for Ti
Resistance for Ti
2004-02-27
aasutosh dave
2004-02-27
Greg Miller
Resistance for Ti
aasutosh dave
2004-02-27
Hello,

  I am having problem with Ti resistance bellow thick nitride. The Ti arms
are 0.16 um thick and open at edges.Silicon nitride is then sputtered ~ 1um
on top of it.  Does the thick nitride deposition on top of Ti affect its
resistance or affect its charateristic? The Ti arm lenght is ~ 200 um.


Thanks,

Aasutosh Dave


NanoFab Center
Arlington, Texas

_________________________________________________________________
Store more e-mails with MSN Hotmail Extra Storage – 4 plans to choose from!
http://click.atdmt.com/AVE/go/onm00200362ave/direct/01/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review
Mentor Graphics Corporation