A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: adhesive based wafer bonding
adhesive based wafer bonding
2004-03-04
BRAD JOHNSON
2004-03-04
Loren St. Clair
2004-03-05
Brubaker Chad
adhesive based wafer bonding
Loren St. Clair
2004-03-04
Robert,

BCB has been successfully used to bond wafers in both full coat and patterned
configurations.  To start I would suggest performing an Internet search using
"BCB" and "BONDING" as key words.  I found some of the same references I used to
set up my BCB bonding process.

Hope this helps,

Loren St. Clair

 -----Original Message-----
From:   Robert Dean [mailto:[email protected]]
Sent:   Thursday, March 04, 2004 8:01 AM
To:     General MEMS discussion
Subject:        [mems-talk] adhesive based wafer bonding

Hello,

Does anyone know which adhesives have been successfully used to bond
silicon wafers together, in place of fusion, anodic, gold thermocompression
or eutectic solder wafer bonding?

Sincerely,

Robert Dean
Auburn University


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation