MEMSnet Home: MEMS-Talk: Resistivity measurment thin film, van der Pauw
Resistivity measurment thin film, van der Pauw
2004-03-04
Stefan Junge
2004-03-04
Juan Pablo Saenz
2004-03-04
Rajesh R
Resistivity measurment thin film, van der Pauw
Rajesh R
2004-03-04
Hoi Stefan,

The link to the NIST  home page should help. It gives you not only the
theory behind resistivity measurement but also the specifications
on how the measurement has to be carried out (clover leaf structure).


http://www.eeel.nist.gov/812/effe.htm#vand


greetings,

Rajesh


______________________________

>From: "Stefan Junge" 
>Reply-To: General MEMS discussion 
>To: 
>Subject: [mems-talk] Resistivity measurment thin film, van der Pauw
>Date: Thu, 4 Mar 2004 17:05:51 +0100
>
>hello,
>
>does anybody know a book or paper where the theory of
>van der Pauw structures is described? I want to measure
>the thin film resistivity and need more information about
>the van der pauw structures or the "cloverleaf" structure?
>
>Regards,
>S. Junge
>
>
>--
>Institute for Microsensors, -actuators and -systems (IMSAS)
>University of Bremen
>Dipl.-Ing. Stefan Junge (Ph.D student)
>Dep. 1: Physics/Electrical Engineering
>Otto-Hahn-Allee
>28359 Bremen, Germany
>
>P.O. Box 330 440
>28334 Bremen, Germany
>
>Tel.: +49-421-218-3586
>Fax.: +49-421-218-4774
>E-Mail: sjunge(at)imsas.uni-bremen.de
>Internet: www.imsas.uni-bremen.de
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Play online games with your friends with MSN Messenger
http://messenger.msn.nl/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing