MEMSnet Home: MEMS-Talk: Polyimide vs HF
Polyimide vs HF
2004-03-08
li Yu
2004-03-09
C.Y. Hsieh
Polyimide vs HF
li Yu
2004-03-08
Dear All:
I plan to coat Cr and Au on silicon and than put it in conc.HF for 30min, now I
find some problem. now I plan to coat layer of polyimide on Au before HF as a
protecting layer
1. the adhension of polyimide to Au is good enough?
2. if the polymide is fully cured, can I  get  rid of it by oxygen plasm?
Thanks in advance!
Lili



---------------------------------
Do you Yahoo!?
Yahoo! Search - Find what you’re looking for faster.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation