A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Coupling Simulation in ANSYS
Coupling Simulation in ANSYS
2004-02-22
Y.C. Lin
2004-02-24
mahdi bagheri
2004-03-09
Hervé LEBLOND
2004-02-25
Daniel Shaw
Coupling Simulation in ANSYS
Hervé LEBLOND
2004-03-09
Dear all

I use Clariant AZ4562 as molds or sacrificial layer.
The problem is that AZ seems to be dissolved in the gold electrolytic
solution.
Do anyone have an idea about the problem?

Thank you for your answering.
Hervé



reply