Hello all,

I'm trying to extend PFA Teflon handles for 3" carriers for use in 6"
chemical bathes.  The largest handles that Flouroware sells would force me
to put my hand into the solution or drop the carrier a few inches.  I'd
still need to retrieve it though and dropping it may crack wafers.

Does anyone know of anyone who could weld extensions on the handles I
have to make them long enough?

Thanks in advance,

Mike

Michael H. Beggans
New Jersey Institute of Technology (NJIT)
[email protected]
973-642-7738 voice
973-596-5794 fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
The Branford Group