Hi Mike,

    I use contact exposure. The intensity of the lamp is 10 mW/cm2 and I
expose for 45 seconds. I typically clean the wafers with acetone and
isopropanol and dry with nitrogen.

Sorry I didn't respond sooner. Thanks for your help.