Hi,all
I want to use the electroless plating gold for about
5um heigh , and 10 um feature. Is that possible and
what kinf of electroless plating solution is
recommended?
Thanks

 P.S. Please reply directly to me email address and
not to the entire MEMS TALK list.  Thank you.





__________________________________
Do you Yahoo!?
Yahoo! Photos: High-quality 4x6 digital prints for 25ยข
http://photos.yahoo.com/ph/print_splash


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering