BCB like resist with low curing temperature
2004-05-18
Olivier Boulle
2004-05-24
Olivier Boulle
BCB like resist with low curing temperature
Olivier Boulle
2004-05-18
Hi,
I am looking for a resist with good planarization properties, low
thermal expansion (CTE), high resistivity,  good adherence of metals
(like BCB) but with  low curing temperature ( typically T<150°). Please
let me know if you heard about such a resist.
Thanks!
Best regards,
Olivier Boulle



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics