MEMSnet Home: MEMS-Talk: Ph diffusion problem
Ph diffusion problem
2004-06-04
Jin Zheng
Ph diffusion problem
Jin Zheng
2004-06-04
Hi,

I have a problem with Ph diffusion. I used 1um thick thermal oxide as
masking material for Ph diffusion. The predeposition was run at 900C for
one hour and the drive was run at 1100C for half hour. However, I found
out that oxide peeled off at the edge of the pattern during the process
and caused lateral Ph diffusion underneath the oxide pattern.  Does
anyone know the cause of the peeling problem and the proper way to do
the Ph diffusion?

Thanks,

Jin

--

Jin Zheng
Michigan Technological University
121 EERC Building, 1400 Townsend Dr.
Houghton, MI 49931






reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer