A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photoresist removal after ion milling
Wafer bonding
2004-06-16
Andrea Tombros
2004-06-16
Aaron M. Cooke
Wafer bonding with glass
2004-06-17
Kirt Williams
Photoresist removal after ion milling
2004-06-17
Robert Dean
2004-06-17
Brent Garber (2 parts)
Photoresist removal after ion milling
Brent Garber
2004-06-17
Dear Robert,

I'm sure you must have a reason for using NMP.  People tend to use it as an
acetone replacement to reduce fire hazards and it is reclaimable.  No one uses
it because it works so well.
Can you use any common resist strippers or EKC's nophenol 922?

Brent

Robert Dean wrote:

> Hello,
>
> We are ion milling a thin layer of Au/Cu on a polymeric substrate, while
> using photoresist (AZ5124EIR) as the etch mask.  The ion milling works very
> well for etching the Au and Cu.  However, the process results in
> crosslinking of the photoresist where we cannot remove it from the
> remaining Au/Cu traces on the substrate, even through heated NMP based
> stripper baths for 20 hours.  Unfortunately, ashing would damage the
> polymeric substrate.  Does anyone have a suggestion on how to remove the
> remaining photoresist?
>
> Sincerely,
>
> Robert Dean
> Auburn University
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 344 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing