MEMSnet Home: MEMS-Talk: KOH Etching - surface roughness of v-groove surfaces
KOH Etching - surface roughness of v-groove surfaces
2004-06-16
Vipul Patel
2004-06-16
Eric Miller
2004-06-17
Kirt Williams
2004-06-17
Robert M Hamilton
KOH Etching - surface roughness of v-groove surfaces
Robert M Hamilton
2004-06-17
Mark Hadley used to bubble O2 through the KOH to reduce H2 bubbles at
the etch surface.

Bill Flounders recently gave me a paper on arsenic and antimony salts to
KOH to produce mirror-like surfaces. Regrettably, I gave him back the
paper.

Bob

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of Kirt Williams
Sent: Thursday, June 17, 2004 10:22 AM
To: General MEMS discussion
Subject: Re: [mems-talk] KOH Etching - surface roughness of v-groove
surfaces

A post-etch processing step that might help you is annealing in hydrogen at
10 Torr, 1100 C, for a few minutes.
This smooths rough silicon surfaces and rounds corners.
This was reported by M.-C. Lee and M. C. Wu from UCLA last week at the
Hilton Head conference.

----- Original Message -----
From: "Vipul Patel" 
To: 
Sent: Wednesday, June 16, 2004 11:22 AM
Subject: [mems-talk] KOH Etching - surface roughness of v-groove surfaces


> Dear MEMS experts,
>
> I  have a need to have a mirror-like surface of the etched V-grooves (
macroscopic) using an-isotropic wet silicon etch.
> When I used conventional KOH etching ( I think it was 40% sol. at 80 deg.
C and a stirrer was used), the resultant surface has several features larger
than 2 micron.( I measured it by cleaving the V-groove and measuring the
surface roughness of the etched surface by dektek profilometer.)
> The crystal plane was aligned to better than 0.05 deg. during lithography
process using an additional mask.
> I came across several papers related to improving the surface roughness,
however being an Electrical Engineer, I do not understand chemical etching
well. Our goal is to have a surface with less than 0.1 micron peak-to-peak
roughness on macroscopic level ( across a few mm long facet)
>
>  Can anyone suggest on what changes should I make to etch process and
share their experience?  Do I have a spec. that is not doable? Eventhough I
have no experience, I can probably also try TMAH or EDP solutions. Also,
does anyone recommend a  MEMS foundry with experience in this specific area.
If they can guarantee the spec. , I can probably give them the entire
device/wafer fabrication.
>
> With best regards,
>
> Vipul Patel..
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing