A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: stress gradient modeling in ANSYS
stress gradient modeling in ANSYS
2004-06-20
Qiao Da Yong
stress gradient modeling in ANSYS
Qiao Da Yong
2004-06-20
the average residual stress polysilicon plate is 11MPa,and the stress gradient
along the depth in 8MPa/um, in order to estimate the stress induced deformation,
some FE analysis is needed, but how can i include the stress gradient and the
average stress in a FEA model(in ANSYS), which command should i use?