annuar
2004-06-21
Michael L
tapered SU-8 structure
Michael L
2004-06-21
Hi Annuar,

I believe the way to do this is to use a grey-scale mask and to conduct
lithography with your SU-8 on a transparent substrate from the bottom up.

Regards,

Michael



>From: "annuar" 
>Reply-To: General MEMS discussion 
>To: 
>Subject: [mems-talk] tapered SU-8 structure
>Date: Mon, 21 Jun 2004 10:17:41 +0800
>
>Dear all,
>
>I'm thinking of making tapered structure on SU-8. SU-8 usually gives a very
>good vertical structured component. However, I wanted to make SU-8
>structure
>to be taper with a certain degree of angle, say 45 degrees. Has anyone ever
>try making such structure using SU-8?
>
>Thanks.
>Abang Annuar Ehsan
>Photonics Tech. Lab
>Institute of Micro Engineering and Nanoelectronics (IMEN)
>Universiti Kebangsaan Malaysia (UKM)

_________________________________________________________________
Use MSN Messenger to send music and pics to your friends
http://www.msn.co.uk/messenger


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing