electroplating Ni on Si
2004-06-23
Chen-Han Lee
2004-06-23
Michael Cooke
electroplating Ni on Si
Chen-Han Lee
2004-06-23

Hi MEMS talk members,

could anyone tell if it is possible
to electroplate Ni onto Si wafer?
If it is, what is the procedure
compare to plating onto say, copper wire?

thanks in advance

chenhan


///////////////////////////////////
Chen-Han Lee
Research Student
School of Manufacturing and Mechanical Engineering,
University of Birmingham,
Birmingham, B15 2TT
United Kingdom,
Phone :  +44 121 4144245
Fax :    +44 121 4143958
E-Mail : [email protected]
///////////////////////////////////



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group