A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AW: Looking for AllResist company
AW: Looking for AllResist company
1998-11-02
Berger, Jürgen
AW: Looking for AllResist company
Berger, Jürgen
1998-11-02
Allresist GmbH
Herr Schirmer
Friedrichshagener Str. 9

12555 Berlin



> -----Ursprüngliche Nachricht-----
> Von:  Claude Beaulieu [SMTP:[email protected]]
> Gesendet am:  Montag, 19. Oktober 1998 16:14
> An:   [email protected]
> Betreff:      Looking for AllResist company
>
>
>
> I'm trying to contact a company that sell a PMMA solution as electron
> beam resist. The company name is AllResist and is located in Berlin,
> Germany.
>
> Does anybody know the phone#, fax#, or e-mail contact for this
> company.
>
> Also if you know other suppliers of PMMA resist, I'm interrested too.
>
> My work involved submicron diffractive optical elements in fused
> silica.
>
>
>
>
> Claude Beaulieu
>
> QPS Technology Inc.
> 2270 St-Francois
> Dorval, Quebec
> H9P 1K2
> Canada
>
> Tel.:514 421 7558 (ext.:32)
> Fax :514 421 7370
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Nano-Master, Inc.