MEMSnet Home: MEMS-Talk: help with PYRALIN 2721
help with PYRALIN 2721
1995-09-26
Dr. Kevin Walsh
1995-10-05
[email protected]
help with PYRALIN 2721
Dr. Kevin Walsh
1995-09-26
We are experimenting with Dupont's PYRALIN 2721 thick photosensitive spin-on
polyimide film and are having problems getting good results. We do not have a
spin development system, and most of the technical info is for spin
development. Does anyone have experience with this product using immersion
development techniques?

Thanks,
Kevin
--
Dr. Kevin M. Walsh
Electrical Engineering Department, Speed Scientific School
University of Louisville, Louisville, KY 40292
(502) 852-0826

Internet address: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group
Addison Engineering