MEMSnet Home: MEMS-Talk: remove Ti from Alu
remove Ti from Alu
2004-07-19
Stephan Biber
2004-07-19
MT Klaus Beschorner
2004-07-20
David Springer
2004-07-22
Jason Viotty
remove Ti from Alu
Stephan Biber
2004-07-19
Hey there,

I have a 2µm thick layer of structured Aluminum on top of a Si-wafer. On
top of the Aluminum there is about 20-30nm of Titanium.

1. Does anyone know how to (chemically?) remove the Titanium without
chaning the size of the Aluminium structures within less than 1µm?
2. I read that the conductivity of sputtered Aluminum can be enhanced by
tempering it. Does anyone know some figures how much the conductivity
changes?

Bes regards,

Stephan

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.