MEMSnet Home: MEMS-Talk: Etchant for both photoresist germanium
Etchant for both photoresist germanium
2004-07-21
[email protected]
Etchant for both photoresist germanium
[email protected]
2004-07-21
Hi, all,

We need transfer pattern on gray level photoresist into germanium. Some
reference mentioned to use H2O2 for germanium wet etching. What I need find out
is an etchant for BOTH gray level photoresist AND germanium. You advice on
which photoresist is well suited for gray level application will also be highy
appreciated. As to photoresist film thickness, it depends on the etch rate
between photoresist and germanium substrate. Can anyone provide any help? Thank
you very much.

Best regard,
Sincerely,
Zhiqiang Liu

--------
Zhiqiang Liu
University of Miami
1251 Memorial Dr, #EB 406
Coral Gables, FL, 33146
Tel: 305-284-5918


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.