Hey,

Freckle or sometimes although named De-Freckle Etch is a mixture of:
Nitric Acid and Ammoniafluoride.
I can give you some typical compositions:
70 Parts per Volume HNO3 69%
1-5 Parts per Volume NH4F solution 40%
25-29 Parts DI-Water

that's it!

Armin