SiO2 etching
2004-08-13
Edi_C
SiO2 etching
Edi_C
2004-08-13
Dear Memsnet members,
I'm looking for theoretical explanation of SiO2 wet etching phenomena in
HF acidand buffered HF in NH4F. It is known that the etching rate of Ge-doped
SiO2 in HF is higher than of pure SiO2 and in the case of ething in bufered HF
the
effect is inverted, i.e. the pure SiO2 is etched faster than Ge-doped SiO2.
I found a couple on papers on this subject but I can't find chemical explanation
enywhere.
Thanks for your help.

Edi


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation