MEMSnet Home: MEMS-Talk: Etching copper in ferric chloride
Etching copper in ferric chloride
2004-08-24
Leidong Mao
2004-08-24
Jauniskis, Linas
Etching copper in ferric chloride
Leidong Mao
2004-08-24
Hello all,
     I have a problem in etching copper with ferric
chloride. The copper(20um) is deposited on a glass
epoxy substrate. Shipley 1813 resist was used to
define the patter and as etching mask, feature size
~60um. The copper substrate was etched in ferric
chloride solution @50C, under microscope it is shown
that some of the pattern was over-etched while others
are untouched.

     The photoresist is around 3um thick(S1813),
exposure dosage ~40mJ/cm2, soft bake for 8 mins@95C,
developed for 100sec, and post develop bake for 30mins
before being put into etchant.

     Any suggestions and help are appreciated. Thanks.

leidong



__________________________________
Do you Yahoo!?
New and Improved Yahoo! Mail - Send 10MB messages!
http://promotions.yahoo.com/new_mail

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.