Jack Peng
copper plating
Jack Peng
2004-08-31
Hi,

      I was using Technic's FB copper bath but the resistivity of the copper
was found to be close to 3 uOhm-cm, while I was expecting something like 2.
I am reading Enthone's Cubath SC data sheet and it looks VERY complicated. I
just want to make some copper inductors and antennas with low resistivity
and smooth surfaces using a simple setup, preferrably just a beaker, a dc
power supply and a couple of wires. Can someone please share a working
recipe?

      Thanks in advance.



Jack




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation