  Dear MEMS-community,

I wonder if anybody of you could give me some information about the
behavior of SU-8
concerning the shrinking (or swelling) subsequent to illumination and PEB.
Guerin 1997 reports a shrinkage of 7.5%.
I have been working with SU-8 for years and my experience is quite
different:
If I measure the surface topography after exposure and PEB I found that
the areas
exposed to UV light are approx. 1% higher than
the surrounding (non-exposed) areas.
This happens regardless of softbake, post exposure bake time and temperature
and overall layer thickness.
What is your experience ?
Many thanks
Peter

--
Vienna University of Technology
Institute of Sensor and Actuator Systems
Gusshausstrasse 27-29/366
A-1040 Vienna
Austria

Tel. +43-1-58801-36643
Fax  +43-1-58801-36699



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.