MEMSnet Home: MEMS-Talk: MF 351 or AZ 351
MF 351 or AZ 351
2004-08-30
Joolien Chee
2004-09-02
Robert Black
2004-09-02
Kasman , Elina
MF 351 or AZ 351
Kasman , Elina
2004-09-02
I agree. For optimal results always use the same manufacturer's
developer as is the resist. Clariant is making AZ resists and
developers. I am not familiar of AZ 351, but Microposit MF 351 developer
concentrate should work very well on 1813 (I only have experience with
1818 and 1811, but they are from the same 1800 PR group, just different
thickness)



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Robert Black
Sent: Thursday, September 02, 2004 4:25 PM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] MF 351 or AZ 351


Did you word this correctly. I think Shiply makes Microposit MF and
Hoechst (also known as AZ) makes the AZ 351.
   Basically the only difference in developers is the surfact used, and
concentration of TMAOH. I would use the Shiply developer on the Shiply
resist. In my opinon, the best developer for Shiply 1813 is Shiply MF
319.



Hi all,

I would like to know what is the difference between Microposit MF 351
and Shipley AZ 351. The target photoresist is Shipley 1813.

Thank you all in advance.

Joolien


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing