thin film metal removal / patterning
2004-09-15
Patrik Möller
2004-09-16
Reiner Witte
2004-09-17
Mark Fuller
2004-09-17
William Lanford-Crick
2004-09-15
[email protected]
2004-09-15
Alex Pozdin (2 parts)
thin film metal removal / patterning
Alex Pozdin
2004-09-15
Date: Wed, 15 Sep 2004 17:09:45 +0200
From: Patrik M?ller 
Subject: [mems-talk] thin film metal removal / patterning
To: 
Message-ID: <002301c49b36$0f447360$9f59a8c0@slimmo>
Content-Type: text/plain;       charset="iso-8859-1"

Does anybody know a way to locally remove a thin gold/titanium film? Say
open up 0.1-1mm diameter holes in a Au/Ti (200/15nm) film on a silicon
wafer without damaging the silicon? The placement accuracy of the holes
need to be +/- 1005m. Regular lithography cannot be used since the film
should remain untouched with polymers. Are there any kinds of laser
processing or similar that can be used? Any ideas?

                      Regards,

                      Patrik


Hello Patrik,
You can do it with Excimer laser micromachining technique. For KrF laser
(wavelength 248nm)I would suggest energy density about 0.4J/cm2. Please,
check our website www.laserusa.com for more information.

Regards,
Alex Pozdin
Alex Pozdin.vcf (text/x-vcard, 416 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing