MEMSnet Home: MEMS-Talk: An epoxy for DRIE
An epoxy for DRIE
2004-09-16
Nicolas Duarte
2004-09-17
Shane Arthur McColman
2004-10-03
Krasniansky Vladimir
An epoxy for DRIE
Nicolas Duarte
2004-09-16
This is a follow up question to a question asked a long time ago (I just
joined the list).
Back in February, Stefan mentioned that he used Aremco Crystal Bond 555 for
bonding two wafers for use in DRIE for through wafer etches.  However when
contacting Aremco they told me that the Crystal Bond series has no thermal
conductivity.  A high thermal conductivity between the wafers is important
for DRIE to achieve high anisotropy since a cool wafer temperature (20 deg
C) has to be maintained.  Our machine also has the ability to do cryo
etching, so the wafer must be at -110 deg C, making high thermal
conductivity even more important.

I have heard of a high thermal conductivity epoxy that is disolvable in
acetone, however I can't seem to find out exactly what it is.  Any suggestions?

Nicolas Duarte


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics