High temperature resistant wax
David Henriks
2004-09-27
We manufacture a wide range of waxes with varying melting points and
solvents.  If you go to our website at www.southbaytech.com and enter
"wax" in the search box it will bring you to a list of waxes that we
offer.  You can download a PDF with a brief description of each one.

Please contact me directly if I can be of additional help.

Best regards-

David

Krasniansky Vladimir wrote:

>Hi Martina,
>  We use WaferGrip (by Dynatex) high temperature glue, it works not bad,
>and resist at least 105 C. NIKKA SEIKO also produces some waxes which
>stand about 100 C, but I didn't try them. Another high temperature wax
>available in Logitech company, but it applied by handily operation.
>  If you get responses with other options, I will glad to hear about
>them.
>
>
>Sincerely,
>
>Vladimir Krasniansky,
>
>Process Engineer,
>
>Gal-El (MMIC);
>
>100, Yitzhak Hanassi Blvd., P.O. Box 330 Ashdod 77102, ISRAEL.
>
>Tel 972-8-857-2436/4
>
>Fax 972-8-857-2658
>
>
>
>
>
>
>
> The information contained in this communication is proprietary to Israel
Aircraft Industries Ltd.
>and/or third parties, may contain confidential or privileged information, and
is intended only for
>the use of the intended addressee thereof. If you are not the intended
addressee, please be aware
>that any use, disclosure, distribution and/or copying of this communication is
strictly prohibited.
>If you receive this communication in error, please notify the sender
immediately and delete it from
>your computer. Thank you.
>
>
>This message is processed by the PrivaWall Email Security Server.
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>
>

--
David Henriks

South Bay Technology, Inc.
1120 Via Callejon
San Clemente, CA 92673 USA

TEL: +1-949-492-2600
Toll-free in the USA: +1-800-728-2233
FAX: +1-949-492-1499

email: [email protected]

Celebrating 40 years of providing Materials Processing Solutions for
Metallogaphy, Crystallography and Electron Microscopy.

Please visit us online at www.southbaytech.com.

The information contained in this message and any attachments is privileged and
confidential.  This message is intended for the individual or entity addressed.
If you are not the intended recipient, please do not read, copy or disclose this
communication.  Notify the sender of the mistake by calling +1-949-492-2600 and
delete this message from your system.





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing