When evaporating gold films (thermal resistive heating or e-beam) on
glass, how does one decrease the roughness of the films? I am using
titanium underlayer while e-beam evaporating and chromium for thermal.
The e-beam made films are better than thermal but not good enough for my
use.
Thanks,SR