micropyramidal hillocks on KOH etched {100} silicon surfaces
2004-10-03
Qing Yao
2004-10-04
Joolien Chee
micropyramidal hillocks on KOH etched {100} silicon surfaces
Joolien Chee
2004-10-04
Hi,

There are plenty of literature which suggest adding chemicals to
prevent formation of hillocks. I suggest Petersen's Bulk Micromachining
review paper.

Best, Joolien


On Oct 3, 2004, at 4:48 PM, Qing Yao wrote:

> Hi,
>
>
> During the KOH etch on {100} silicon surfaces, lots of micropyramid
> hillocks are formatted. I was wondering if there is any effective
> method that can be used to get a smooth and pyramid free etched
> surface. I used 30% w/w KOH and IPA and did the etch at 80C. Please
> let me know if you have any comments or suggestions. Thanks!
>
>
>
> Best Regards,
>
>
> Qing Yao
> ___________________
> M&IE @ UIUC
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.