Photoresist for Patterning Aluminum
2004-10-05
Vivek Mukhatyar
2004-10-05
Shay Kaplan
teflon glue...
2004-10-05
Venkatachalam Chokkalingam
2004-10-05
William Lanford-Crick
2004-10-05
aasutosh dave
2004-10-05
rakesh babu
photopatternable silicone biocompatibility
2004-10-06
[email protected]
2004-10-05
Bill Moffat
Photoresist for Patterning Aluminum
rakesh babu
2004-10-05
hello,

   Lift off would be a better option for this kind of
problems,as you will not be needing any kind of wet
etchant.

 If you prefer sticking by the previous method,I
suggest you hard bake the photoresist at a temperature
of 130 deg C for about 10-15 min. Later i also suggest
that you descum using oxygen plasma.This should work
for you.

Regards,
Rakesh Katragadda
Graduate Researcher
Wayne state university

--- Vivek Mukhatyar  wrote:

> I was trying to spin coat aluminium with shipley
> 1818 negative resist.
>  But when I used a wet etching solution the resist
> wasn't able to
> withstand the etchant.  My patterns are on the scale
> of microns and
> the best way to etch is through wet etching because
> i need to remove
> alomost 300 micron thick aluminum.  Does anyone know
> the steps to spin
> a thick layer of resist that will withstand the
> etchant that is made
> up of Hcl and CuCl2.  I have SU-8 and 1818 to my
> disposal.  I also
> need to remove the resist after the etching process.
>
> Thank you,
>
> Vivek Mukhatyar
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>


__________________________________________________
Do You Yahoo!?
Tired of spam?  Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics