MEMSnet Home: MEMS-Talk: Re: glass-frit
Re: glass-frit
1998-11-20
Shile
Re: glass-frit
Shile
1998-11-20
-----Original Message-----
From: [email protected] 
To: [email protected] 
Date: Monday, November 16, 1998 10:31 PM
Subject: Where to find grass-frit paste?


Glass Frit can be obtained from Ferro Corporation in Clevland Ohio (USA) ,
phone (216) 641 -8580


> I'm a research student at the Technical University of Dresden, Germany,
working at a project
> about glass-frit bonding.
>
> For my practical research I need small amounts of glass-frit paste. Could
you perhaps tell me
> where I could find this, or its components, and how much it would cost me?
Furthermore, I
> would need to know about the conditions this paste fulfills. How does it
react to exposure to
> temperature or pressure? I read about kinds that react at 600C-800C,
others that react at
> about 290C-380C, and yet another reacting at above 100C. Would that be the
same paste
> or are totally different procedures applied?
> I would be very grateful if you could help me out with information,
sources in literature or
> ideas where to look.
>
>
> With best regards
>
> Genadi Genadiev
> [email protected]
>Request: END
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics